TU400 Vis
TU500 UV-VIS
T6V Vis
T6u uv-vis
TU600 UV-VIS
T7 uv-vis
T7S UV-VIS
T7D UV-VIS
TU700 UV-VIS
T7DS UV-VIS
T8DCS UV-VIS
T9DCS UV-VIS
T10DCS UV-VIS
PERANGKAT LUNAK UVWIN 6/GMP
Kit Kualifikasi UV/VIS IQ/OQ/PQ
Ftir8000
Ftir8100
A3F
A3G
A3afg
AA990F
AA990G
AA990AFG
Pf7
FP912-2
FP912-3
FP912-4
FP912-5
AAS IQ/OQ/PQ
XD-2
XD-3
XD-6
M7 quadrupole single gc-ms
G5 GC
GC1100 GC
L600 Cairan Kinerja Tinggi
I-Depot Aman
GBW-1
GWB-1-B
GWB-2
GWB-2-B
Sistem Pencernaan Microwave M40
D70E Labware Washer

Penentuan Kadar Timbal dalam Paduan Aluminium dengan Spektrometri Serapan Atom Nyala Api

1 Method Summary

Wet digestion: dissolve the sample with hydrochloric acid, nitric acid and hydrogen peroxide. Determine at 283.3 nm using air‑acetylene neutral flame.

2 Scope

Applicable to the determination of lead in aluminum alloys.

3 Reference Standard

GB 20975

3 Test Instruments

· Flame Atomic Absorption Spectrophotometer 1 set – Lead hollow cathode lamp

· Acetylene 1 cylinder Purity ≥99.99%

·  Air Compressor 1 set Rated discharge pressure: 0.3 MPa

kontak

Bertemu dengan para profesional

lebih banyak berita

Tinggalkan Pesan
Mari kita ucapkan talkback dari tim profesional kami

Dokumentasi tentang produk akan dipasok melalui email pengembalian jika Anda meninggalkan alamat email Anda.