{"id":3790,"date":"2025-07-28T16:03:51","date_gmt":"2025-07-28T08:03:51","guid":{"rendered":"https:\/\/www.pgeneral.com\/?p=3790"},"modified":"2025-07-28T16:03:51","modified_gmt":"2025-07-28T08:03:51","slug":"determination-of-lead-in-drinking-water-graphite-furnace-atomic-absorption-spectrometry","status":"publish","type":"post","link":"https:\/\/www.pgeneral.com\/es\/applications\/determination-of-lead-in-drinking-water-graphite-furnace-atomic-absorption-spectrometry","title":{"rendered":"Determinaci\u00f3n del plomo en agua potable (espectrometr\u00eda de absorci\u00f3n at\u00f3mica en horno de grafito)"},"content":{"rendered":"<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">1. Resumen del m\u00e9todo<\/h2>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Despu\u00e9s del tratamiento apropiado, la muestra se atomiza en un horno de grafito, y la absorbancia se mide a 283,3 nm. Dentro de un cierto intervalo de concentraci\u00f3n, la absorbancia del plomo es proporcional a su contenido, y la cuantificaci\u00f3n se realiza mediante comparaci\u00f3n con una serie est\u00e1ndar.<\/div>\n<div>\n<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">2. Instrumentos y reactivos<\/h2>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1 Instrumentos y equipos<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1.1 Instrumentos de ensayo<\/h4>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>Nombre<\/th>\n<th>Cantidad<\/th>\n<th>Requisitos t\u00e9cnicos<\/th>\n<th>Accesorios<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Micropipeta<\/td>\n<td>1 cada uno<\/td>\n<td>100 \u03bcL ~ 1000 \u03bcL, 1000 \u03bcL ~ 5000 \u03bcL, 5 ~ 50 \u03bcL<\/td>\n<td><\/td>\n<\/tr>\n<tr>\n<td>Matraz volumetrico<\/td>\n<td>Varios<\/td>\n<td>de 100 ml<\/td>\n<td><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1.2 Equipo de pretratamiento<\/h4>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>N\u00famero de serie.<\/th>\n<th>Nombre<\/th>\n<th>Cantidad<\/th>\n<th>Requisitos t\u00e9cnicos<\/th>\n<th>Accesorios<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Micropipeta<\/td>\n<td>1 cada uno<\/td>\n<td>100 \u03bcL ~ 1000 \u03bcL, 1000 \u03bcL ~ 5000 \u03bcL, 5 ~ 50 \u03bcL<\/td>\n<td><\/td>\n<\/tr>\n<tr>\n<td>2<\/td>\n<td>Matraz volumetrico<\/td>\n<td>Varios<\/td>\n<td>de 100 ml<\/td>\n<td><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.2 Reagentes<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.2.1 Reagentes<\/h4>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>N\u00famero de serie.<\/th>\n<th>Nombre<\/th>\n<th>Requisitos t\u00e9cnicos<\/th>\n<th>Observaciones<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>\u00c1cido n\u00edtrico<\/td>\n<td>Grado MOS<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.3 Normas de referencia<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.3.1 Soluciones de stock<\/h4>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>N\u00famero de serie.<\/th>\n<th>\u00a1No! No!<\/th>\n<th>Nombre<\/th>\n<th>Requisitos t\u00e9cnicos<\/th>\n<th>Observaciones<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>GBW 08619<\/td>\n<td>Substancia est\u00e1ndar de soluci\u00f3n de plomo de un solo elemento<\/td>\n<td>1000 \u03bcg\/ml<\/td>\n<td>Instituto Nacional de Metrolog\u00eda, China<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">3. Procedimientos operacionales<\/h2>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">3.1 Procesamiento de muestras<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">3.1.1 Preparaci\u00f3n de la soluci\u00f3n de ensayo<\/h4>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Tome 100 ml de muestra de agua en un matraz volum\u00e9trico, agregue 0,5 ml de \u00e1cido n\u00edtrico y mezcle bien. Realice una prueba en blanco junto a la muestra.<\/div>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">3.1.2 Preparaci\u00f3n de soluciones est\u00e1ndar<\/h4>\n<ol class=\"auto-hide-last-sibling-br\">\n<li>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Preparaci\u00f3n de la soluci\u00f3n intermedia est\u00e1ndar de plomo: soluci\u00f3n est\u00e1ndar de plomo (1,0 \u03bcg\/ml): pipeta con precisi\u00f3n 0,1 ml de soluci\u00f3n est\u00e1ndar de plomo (1000 \u03bcg\/ml) en un matraz volum\u00e9trico de 100 ml, agrega 0,5 ml de soluci\u00f3n de \u00e1cido n\u00edtrico, diluye hasta la marca y agite bien.<\/div>\n<\/li>\n<li>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Preparaci\u00f3n de la serie est\u00e1ndar de plomo: Pipeta con precisi\u00f3n 0,0, 0,1, 0,2, 0,3 y 0,4 ml de soluci\u00f3n est\u00e1ndar de plomo (1,0 \u03bcg\/ml) en matraces volum\u00e9tricos de 10 ml respectivamente. A\u00f1adir 0,5 ml de soluci\u00f3n de \u00e1cido n\u00edtrico a cada uno, diluir hasta la marca, y obtener soluciones de serie est\u00e1ndar de plomo con concentraciones de 0,0, 10,0, 20,0, 30,0 y 40,0 ng\/ml.<\/div>\n<\/li>\n<\/ol>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">3.2 Prueba de muestras<\/h3>\n<ol class=\"auto-hide-last-sibling-br\">\n<li>Condiciones de ensayo Condiciones de referencia para la detecci\u00f3n con espectrofot\u00f3metro de absorci\u00f3n at\u00f3mica en horno de grafito<\/li>\n<\/ol>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>Elemento<\/th>\n<th>Plomo<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>Longitud de onda (nm)<\/td>\n<td>283.3<\/td>\n<\/tr>\n<tr>\n<td>Ancho de banda espectral (nm)<\/td>\n<td>0.4<\/td>\n<\/tr>\n<tr>\n<td>Corriente de la l\u00e1mpara del elemento (mA)<\/td>\n<td>2.0<\/td>\n<\/tr>\n<tr>\n<td>M\u00e9todo de correcci\u00f3n de fondo<\/td>\n<td>L\u00e1mpara de deuterio<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>&nbsp;<\/p>\n<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\"><strong>Programa de Calentamiento de Horno de Grafito<\/strong><\/div>\n<p>&nbsp;<\/p>\n<div class=\"auto-hide-last-sibling-br table-container-GhL7Lo\">\n<table>\n<thead>\n<tr>\n<th>Paso<\/th>\n<th>Procedimiento<\/th>\n<th>Temperatura (\u2103)<\/th>\n<th>Tiempo de rampa (s)<\/th>\n<th>Tiempo de espera (s)<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Secado<\/td>\n<td>120<\/td>\n<td>10<\/td>\n<td>10<\/td>\n<\/tr>\n<tr>\n<td>2<\/td>\n<td>Ashing<\/td>\n<td>450<\/td>\n<td>10<\/td>\n<td>10<\/td>\n<\/tr>\n<tr>\n<td>3<\/td>\n<td>Atomizaci\u00f3n<\/td>\n<td>1800<\/td>\n<td>0<\/td>\n<td>2<\/td>\n<\/tr>\n<tr>\n<td>4<\/td>\n<td>Limpieza<\/td>\n<td>1900<\/td>\n<td>1<\/td>\n<td>2<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p>&nbsp;<\/p>\n<ol class=\"auto-hide-last-sibling-br\" start=\"2\">\n<li>Ensayo de muestras Determinar la absorbancia de soluciones est\u00e1ndar, soluciones de prueba en blanco y soluciones de prueba en secuencia. Retire la absorbancia de la soluci\u00f3n est\u00e1ndar cero de la absorbancia de cada soluci\u00f3n est\u00e1ndar. Trace una curva de trabajo con la concentraci\u00f3n de masa como abscisa y la absorbancia correspondiente como ordenada. En funci\u00f3n de la absorbancia medida de la soluci\u00f3n de ensayo, encuentra la concentraci\u00f3n en masa de plomo de la curva de trabajo.<\/li>\n<\/ol>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">3.3 C\u00e1lculo de resultados<\/h3>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">F\u00f3rmula:<\/div>\n<p><img decoding=\"async\" class=\"alignnone  wp-image-3791\" src=\"http:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/07\/2222\u5fae\u4fe1\u56fe\u7247_20250728160213_3807-300x128.png\" alt=\"\" width=\"199\" height=\"85\" srcset=\"https:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/07\/2222\u5fae\u4fe1\u56fe\u7247_20250728160213_3807-300x129.png 300w, https:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/07\/2222\u5fae\u4fe1\u56fe\u7247_20250728160213_3807-18x8.png 18w, https:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/07\/2222\u5fae\u4fe1\u56fe\u7247_20250728160213_3807.png 303w\" sizes=\"(max-width: 199px) 100vw, 199px\" \/><\/p>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">D\u00f3nde:<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">\u03c1 \u2014 Concentraci\u00f3n en masa de plomo en la muestra de agua, en miligramos por litro (mg\/L);<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\"><span class=\"container-rkuXQi math-inline\" data-custom-copy-text=\"\\(\\rho_1\\)\">\u03c11<\/span>Concentraci\u00f3n en masa de plomo en la muestra de agua obtenida a partir de la curva est\u00e1ndar, en nanogramos por mililitro (ng\/ml);<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\"><span class=\"container-rkuXQi math-inline\" data-custom-copy-text=\"\\(V_1\\)\">V1<\/span>\u00a0Volumen de la soluci\u00f3n de muestra para la determinaci\u00f3n, en mililitros (ml);<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\"><span class=\"container-rkuXQi math-inline single-Z69glH\" data-custom-copy-text=\"V\">V<\/span>\u00a0Volumen de la muestra de agua original, en mililitros (ml);<\/div>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">1000 - Factor de conversi\u00f3n.<\/div>\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>1. Method Overview After appropriate treatment, the sample is atomized in a graphite furnace, and the absorbance is measured at 283.3 nm. Within a certain concentration range, the absorbance of lead is proportional to its content, and quantification is performed by comparison with a standard series. 2. Instruments and Reagents 2.1 Instruments and Equipment 2.1.1 [&hellip;]<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[36,73],"tags":[],"class_list":["post-3790","post","type-post","status-publish","format-standard","hentry","category-applications","category-food-and-drugs"],"acf":[],"_links":{"self":[{"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/posts\/3790","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/comments?post=3790"}],"version-history":[{"count":0,"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/posts\/3790\/revisions"}],"wp:attachment":[{"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/media?parent=3790"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/categories?post=3790"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.pgeneral.com\/es\/wp-json\/wp\/v2\/tags?post=3790"}],"curies":[{"name":"WP","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}