{"id":3902,"date":"2025-09-04T11:03:47","date_gmt":"2025-09-04T03:03:47","guid":{"rendered":"https:\/\/www.pgeneral.com\/?p=3902"},"modified":"2025-09-04T11:03:47","modified_gmt":"2025-09-04T03:03:47","slug":"determination-of-copper-in-graphite-powder-flame-atomic-absorption-spectrometry-2","status":"publish","type":"post","link":"https:\/\/www.pgeneral.com\/de\/applications\/determination-of-copper-in-graphite-powder-flame-atomic-absorption-spectrometry-2","title":{"rendered":"Bestimmung von Kupfer in Graphitpulver (Flammenatomatorenabsorptionsspektrometrie)"},"content":{"rendered":"<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">1. Methodenblick<\/h2>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Nach dem Verdauen der Probe mit Aqua Regia wird die Bestimmung mit einer Luft-Acetylenflamme bei einer Instrumentwellenl\u00e4nge von 324,7 nm durchgef\u00fchrt.<\/div>\n<div>\n<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">2. Instrumente und Reagentien<\/h2>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1 Instrumente und Ausr\u00fcstung<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1.1 Pr\u00fcfinstrumente<\/h4>\n<div class=\"auto-hide-last-sibling-br mdbox-table-root table-container-GhL7Lo\" data-scroll-inline-overflow=\"true\" data-scroll-inline-at-start=\"true\" data-scroll-inline-start-overflow=\"false\" data-scroll-inline-at-end=\"false\" data-scroll-inline-end-overflow=\"true\">\n<div class=\"table-scroll-container-hgHkfW mdbox-table-scroll-container\">\n<table>\n<thead>\n<tr>\n<th>Seriennummer.<\/th>\n<th>Name<\/th>\n<th>Menge<\/th>\n<th>Technische Anforderungen<\/th>\n<th>Zubeh\u00f6r<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Flammenabsorptionsspektrophotometer<\/td>\n<td>1 Satz<\/td>\n<td>&#8211;<\/td>\n<td>Kupfer Hohlkathodenlampe<\/td>\n<\/tr>\n<tr>\n<td>2<\/td>\n<td>Acetylengas<\/td>\n<td>1 Zylinder<\/td>\n<td>Reinheit \u2265 99,99%<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>3<\/td>\n<td>Luftkompressor<\/td>\n<td>1 Satz<\/td>\n<td>Nennleistungsdruck: 0,3 MPa<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/div>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.1.2 Probenvorbehandlungsausr\u00fcstung<\/h4>\n<div class=\"auto-hide-last-sibling-br mdbox-table-root table-container-GhL7Lo\" data-scroll-inline-overflow=\"true\" data-scroll-inline-at-start=\"true\" data-scroll-inline-start-overflow=\"false\" data-scroll-inline-at-end=\"false\" data-scroll-inline-end-overflow=\"true\">\n<div class=\"table-scroll-container-hgHkfW mdbox-table-scroll-container\">\n<table>\n<thead>\n<tr>\n<th>Seriennummer.<\/th>\n<th>Name<\/th>\n<th>Menge<\/th>\n<th>Technische Anforderungen<\/th>\n<th>Zubeh\u00f6r<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Temperaturgesteuerte Hei\u00dfplatte<\/td>\n<td>1 Satz<\/td>\n<td>Nenntemperatur: Raumtemperatur ~ 300 \u2103<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>2<\/td>\n<td>Elektronische Balance<\/td>\n<td>1 Satz<\/td>\n<td>Empfindlichkeit: 0,1 mg<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>3<\/td>\n<td>Ultrareines Wassersystem<\/td>\n<td>1 Satz<\/td>\n<td>&#8211;<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>4<\/td>\n<td>Mikropipette<\/td>\n<td>1 jedes<\/td>\n<td>Bereiche: 20 \u03bcL ~ 200 \u03bcL, 100 \u03bcL ~ 1000 \u03bcL<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>5<\/td>\n<td>Volumetrische Flasche<\/td>\n<td>Mehrere<\/td>\n<td>Volumen: 100 ml<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>6<\/td>\n<td>Testrohr<\/td>\n<td>Mehrere<\/td>\n<td>Volumen: 25 ml<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/div>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.2 Reagenzien<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.2.1 Rohreagenzien<\/h4>\n<div class=\"auto-hide-last-sibling-br mdbox-table-root table-container-GhL7Lo\" data-scroll-inline-overflow=\"false\" data-scroll-inline-at-start=\"true\" data-scroll-inline-start-overflow=\"false\" data-scroll-inline-at-end=\"true\" data-scroll-inline-end-overflow=\"false\">\n<div class=\"table-scroll-container-hgHkfW mdbox-table-scroll-container\">\n<table>\n<thead>\n<tr>\n<th>Seriennummer.<\/th>\n<th>Name<\/th>\n<th>Technische Anforderungen<\/th>\n<th>Anmerkungen<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Stickstoffs\u00e4ure<\/td>\n<td>MOS-Klasse<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<tr>\n<td>2<\/td>\n<td>Salzs\u00e4ure<\/td>\n<td>Garantiertes Reagenz (GR)<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/div>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.2.2 Vorbereitete Reagenzien<\/h4>\n<div class=\"auto-hide-last-sibling-br mdbox-table-root table-container-GhL7Lo\" data-scroll-inline-overflow=\"false\" data-scroll-inline-at-start=\"true\" data-scroll-inline-start-overflow=\"false\" data-scroll-inline-at-end=\"true\" data-scroll-inline-end-overflow=\"false\">\n<div class=\"table-scroll-container-hgHkfW mdbox-table-scroll-container\">\n<table>\n<thead>\n<tr>\n<th>Seriennummer.<\/th>\n<th>Name<\/th>\n<th>Herstellungsmethode<\/th>\n<th>Anmerkungen<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>Stickstoffs\u00e4urel\u00f6sung (1 99)<\/td>\n<td>10 ml Salpeters\u00e4ure messen, langsam zu 990 ml deionisiertes Wasser hinzuf\u00fcgen und gut mischen.<\/td>\n<td>&#8211;<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/div>\n<h3 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.3 Referenzstandards<\/h3>\n<h4 class=\"header-vfC6AV auto-hide-last-sibling-br\">2.3.1 Lagerl\u00f6sung<\/h4>\n<div class=\"auto-hide-last-sibling-br mdbox-table-root table-container-GhL7Lo\" data-scroll-inline-overflow=\"true\" data-scroll-inline-at-start=\"true\" data-scroll-inline-start-overflow=\"false\" data-scroll-inline-at-end=\"false\" data-scroll-inline-end-overflow=\"true\">\n<div class=\"table-scroll-container-hgHkfW mdbox-table-scroll-container\">\n<table>\n<thead>\n<tr>\n<th>Seriennummer.<\/th>\n<th>- Nein. - Nein.<\/th>\n<th>Name<\/th>\n<th>Technische Anforderungen<\/th>\n<th>Anmerkungen<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td>1<\/td>\n<td>GBW 08615<\/td>\n<td>Kupfer-Einelement-Standardl\u00f6sung<\/td>\n<td>Konzentration: 1000 \u03bcg\/ml<\/td>\n<td>Nationales Institut f\u00fcr Metrologie, China<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<\/div>\n<h2 class=\"header-vfC6AV auto-hide-last-sibling-br\">3. Ergebnisberechnung<\/h2>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Der Kupfergehalt in der Probe wird anhand der folgenden Formel berechnet:<\/div>\n<div><img decoding=\"async\" class=\"alignnone size-full wp-image-3903\" src=\"http:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/09\/555.png\" alt=\"\" width=\"201\" height=\"51\" srcset=\"https:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/09\/555.png 201w, https:\/\/www.pgeneral.com\/wp-content\/uploads\/2025\/09\/555-18x5.png 18w\" sizes=\"(max-width: 201px) 100vw, 201px\" \/><\/div>\n<p><br class=\"container-utlnW2 wrapper-d0Cc1k undefined\" \/><\/p>\n<div class=\"auto-hide-last-sibling-br paragraph-JOTKXA paragraph-element br-paragraph-space\">Wo:<\/div>\n<ul class=\"auto-hide-last-sibling-br\">\n<li><span class=\"container-rkuXQi math-inline single-Z69glH\" data-custom-copy-text=\"X\">X<\/span>\u00a0= Kupfergehalt in der Probe, Einheit: Milligramm pro Kilogramm (mg\/kg);<\/li>\n<li>\u03c1 = Massenkonzentration von Kupfer in der Probentestl\u00f6sung, Einheit: Mikrogramm pro Milliliter (\u03bcg\/ml);<\/li>\n<li><span class=\"container-rkuXQi math-inline\" data-custom-copy-text=\"\\(\\rho_{0}\\)\">\u03c10<\/span>= Massenkonzentration von Kupfer in der Rohl\u00f6sung, Einheit: Mikrogramm pro Milliliter (\u03bcg\/ml);<\/li>\n<li><span class=\"container-rkuXQi math-inline single-Z69glH\" data-custom-copy-text=\"f\">F<\/span>\u00a0= Verd\u00fcnnungsfaktor der verdauten Probenl\u00f6sung;<\/li>\n<li><span class=\"container-rkuXQi math-inline single-Z69glH\" data-custom-copy-text=\"V\">V<\/span>\u00a0= Gesamtvolumen der verdauten Probenl\u00f6sung, Einheit: Milliliter (mL);<\/li>\n<li><span class=\"container-rkuXQi math-inline single-Z69glH\" data-custom-copy-text=\"m\">M<\/span>\u00a0= Masse der Probe, Einheit: Gramm (g).<\/li>\n<\/ul>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>1. Method Overview After the sample is digested with aqua regia, the determination is carried out using an air-acetylene flame at an instrument wavelength of 324.7 nm. 2. Instruments and Reagents 2.1 Instruments and Equipment 2.1.1 Testing Instruments Serial No. Name Quantity Technical Requirements Accessories 1 Flame Atomic Absorption Spectrophotometer 1 set &#8211; Copper Hollow [&hellip;]<\/p>\n","protected":false},"author":2,"featured_media":0,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[81,36],"tags":[],"class_list":["post-3902","post","type-post","status-publish","format-standard","hentry","category-petrochemical-and-chemical","category-applications"],"acf":[],"_links":{"self":[{"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/posts\/3902","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/comments?post=3902"}],"version-history":[{"count":0,"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/posts\/3902\/revisions"}],"wp:attachment":[{"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/media?parent=3902"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/categories?post=3902"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.pgeneral.com\/de\/wp-json\/wp\/v2\/tags?post=3902"}],"curies":[{"name":"WP","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}